EN 80 Cr V 2 Structural and constructional steels
Data updates
This material has 192 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
EN 80 Cr V 2 Chemical Composition
EN 10132-4: 2000 / Cold rolled narrow steel strip for heat treatment - Technical delivery conditions - Part 4: Spring steels and other applications
Looking for full material performance data?
Free registration required • Instant access
EN 80 Cr V 2 Physical Properties
Temperature
This material has 192 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
EN 80 Cr V 2 Heat Treatments
- Austenitizing: 840-870°C, cooling in oil.
- Austenitized at 840-870°C, quenched in oil.
EN 80 Cr V 2 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
91 Cross References
-
19 Composition
-
18 Mechanical Properties
-
3 Physical Properties
-
5 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
56 Total Suppliers