DIN 75 Cr 1 Tool steels
Material group:
Ferrous Alloys / Tool steels, Ferrous Alloys / Structural and constructional steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2021-12
Total number of updates: 1
Update History
This material has 166 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
DIN 75 Cr 1 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.7000 – 0.8000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.3000 – 0.4000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.6000 – 0.8000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
DIN 17350: 1980 / Tool Steels; Technical Conditions of Delivery
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
DIN 75 Cr 1 Physical Properties
Temperature
Modulus of Elasticity
190 — 210
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.67 — 8
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access
View Complete Material Data
This material has 166 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
DIN 75 Cr 1 Heat Treatments
- Operation of hardening - 770-800°C; Hardness, Brinell, HB 30 < 200; Hardness HRc 66; Hot working 1000-800°C; Soft annealing 700-720°C; Temper 180-200°C
- Austenitized at 810-840°C, quenched in oil.
DIN 75 Cr 1 Mechanical Properties
Temperature
Yield Strength, Rp0.2
≤ 550
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Tensile Strength
690
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
13
%
Unlock full details
Full data available with free access
View Complete Material Data
Rockwell Hardness (HR)
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
Vickers Hardness (HV)
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
85 Cross References
-
13 Composition
-
10 Mechanical Properties
-
6 Physical Properties
-
2 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
50 Total Suppliers