GS-25CrMo4 (Germany / DIN) Material Properties

Other designations:
Material group: Ferrous Alloys / Cast steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2024-05
Total number of updates: 3
Update History:
2019-06 2016-04

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 300 MPa view details
Tensile Strength 550 — 900 MPa view details
Elongation, A 10 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 43.5 ksi view details
Tensile Strength 79.8 — 130.5 ksi view details
Elongation, A 10 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.2200 – 0.2900
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.8000 – 1.2000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.5000 – 0.8000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

DIN 17205: 1992 / Quenched and tempered steel castings for general applications; technical delivery conditions

Heat Treatments

  • Air Quenched and Tempered Hardening: 880-950°C; Tempering: 600-650°C Liquid Quenched and Tempered (I) Hardening: 880-950°C; Tempering: 600-650°C Liquid Quenched and Tempered (II) Hardening: 880-950°C; Tempering: 550-600°C