DIN 1.7221 Cast steels
Material group:
Ferrous Alloys / Cast steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: -
Total number of updates: 0
Update History
—
This material has 437 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
DIN 1.7221 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.22 – 0.29
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.80 – 1.20
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
EN 10293: 2015 / Steel castings for general engineering uses
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
This material has 437 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
DIN 1.7221 Heat Treatments
- Quenced and tempered: (+QT1) quenched from 880 to 950°C, cooled in liquid or air (for information only) and temped from 600 to 650°C;
(+QT2) quenched from 880 to 950°C, cooled in liquid (for information only) and tempered from 550 to 600°C.
DIN 1.7221 Mechanical Properties
Temperature
Yield Strength, Rp0.2
300
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Tensile Strength
550 — 850
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
10
%
Unlock full details
Full data available with free access
View Complete Material Data
Impact Energy
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
234 Cross References
-
10 Composition
-
12 Mechanical Properties
-
- Physical Properties
-
1 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
180 Total Suppliers