11 CrMo 9-10 (Germany / DIN) Material Properties
Other designations:
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2024-04
Total number of updates: 6
Update History:
2021-09
2020-02
2017-06
2017-05
2014-04
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.08 – 0.15
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
2.00 – 2.50
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.25
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
N
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
EN 10222-2: 2017 / Steel forgings for pressure purposes - Part 2: Ferritic and martensitic steels with specified elevated temperature properties
Heat Treatments
- Austenitized: 920 - 980°C; Tempered: 650 - 750°C.
- N+T/QA/QL - Normalized and Tempered or Air Quenched or Liquid Quenched. <br />QL - Liquid Quenched.<br />Austenitizing: 920-980°C;<br />Tempering: 670-750°C.
-
179 Cross References
-
37 Composition
-
80 Mechanical Properties
-
3 Physical Properties
-
4 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
3 Creep
-
28 Joints
-
- Coatings
-
154 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
142 Total Suppliers