DIN 1.7262 Structural and constructional steels
Data updates
This material has 276 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.7262 Chemical Composition
Longhai Steel Co., Ltd, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
DIN 1.7262 Physical Properties
Temperature
This material has 276 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.7262 Heat Treatments
- Hot working 1050-850°C; Soft annealing 680-700°C; Case Hardening - Double hardening Carburize 840-880°C; Cooling after case hardening - oil or water Intermediate annealing 650-680°C Surface hardening 810-830°C Tempering 150-180°C, duration 1h
DIN 1.7262 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 1.7262 International Equivalent Materials
Showing 15 of 120 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 120 international equivalents?
See all 120 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 120Cross References
- 7Composition
- 11Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- 2Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 29Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 103Total Suppliers