PROPRIETARY TENAX300 工具钢
材料组别:
黑色金属 / 工具钢
国家与地区/标准:
PROPRIETARY
数据更新
最新更新: 2022-01
更新总数: 1
更新历史
PROPRIETARY TENAX300 化学成分
化学元素
数值
单位
CAS 编号
Villares Metals, Product Data Sheets,
需要完整的材料性能数据吗?
查看完整材料数据 ›
需要注册 • 立即访问
需要注册 • 立即访问
PROPRIETARY TENAX300 物理性能
PROPRIETARY TENAX300 热处理
- Stress relief: The procedure employs slowly heating to 500-600°C and furnace cooling until 200°C. After tooling, the stress relief must employ a temperature 50°C lower than that of the last tempering.
Hardening: Preheat tools at 780/820°C and transfer them to another furnace hold at 1000/1040°C.
Cooling:
a) Salt-bath at 500/550°C.
b) Oil
c) Forced air.
Tempering: Tools must be tempered immediately after hardening, as soon as they reach 60°C. It is necessary, at least, triple tempering; after each tempering, tools must be slowly cooled to room temperature. The first tempering treatment should be performed at 540°C, and the other treatments between 540-650°C, depending on the desired hardness.
Nitriding: Nitriding must be employed after hardening and tempering, normally in temperatures between 500 and 550°C, since they are at least 50°C lower than the last tempering temperature. As the surface finishing influence the nitriding layer efficiency, it is recommended that the surface is carefully grinned and polished before the nitriding process.
PROPRIETARY TENAX300 机械性能
PROPRIETARY TENAX300 的全球近似对照材料
显示 1 条结果,共计 1 条。
材料牌号
标准
国家与地区 / 生产商
近似类型
近似对照材料反映了不同材料间化学成分的相似性和力学性能的相似性——请务必根据具体应用场景的适用标准和条件具体核实材料的适用性。
根据您的应用场景优化材料选择 - 预约演示
- 1交叉引用
- 5化学成分
- 1机械性能
- 13物理性能
- 2热处理
- -金相组织
- -切削加工性能
- -应力-应变
- -成形性能
- -疲劳
- -断裂
- -爬行
- -焊接接头
- -涂层
- -尺寸
- -摩擦学
- -腐蚀
- -老化
- -耐候性
- -辐照
- 2供应商总数