PROPRIETARY BÖHLER E200 结构钢
材料组别:
黑色金属 / 结构钢
国家与地区/标准:
PROPRIETARY
数据更新
最新更新: 2021-01
更新总数: 1
更新历史
PROPRIETARY BÖHLER E200 化学成分
化学元素
数值
单位
CAS 编号
Böhler Edelstahl, Product Data Sheets,
需要完整的材料性能数据吗?
查看完整材料数据 ›
需要注册 • 立即访问
需要注册 • 立即访问
PROPRIETARY BÖHLER E200 物理性能
温度
PROPRIETARY BÖHLER E200 热处理
- Normalizing:
850 to 880°C / Air cooling
Carburising:
880 to 980°C; The following criteria must be considered when selecting the carburising temperature; the desired carburising time; the chosen carburising medium and available carburising equipment; the intended process and the required microstructure. When direct hardening, carburising is generally carried out below 950°C. Carburising temperatures up to over 1000°C are used in special cases.
Cooling from case hardening temperature:
Oil, water (Quenching in water for large components of simple shapes only)
Salt bath (160 - 250°C).
Intermediate annealing:
620 to 650°C / Cooling in furnace
Core hardening: 840 to 880°C / Oil, water (Quenching in water for large components of simple shapes only)
salt bath (160 - 250°C);
Case hardening: 780 to 820°C / Oil, water (Quenching in water for large components of simple shapes only)
Salt bath (160 - 250°C);
Tempering:
150 to 200°C
PROPRIETARY BÖHLER E200 机械性能
PROPRIETARY BÖHLER E200 国际等效材料
显示 15 / 72 条结果。
材料牌号
标准
国家与地区 / 生产商
近似类型
等效类别反映化学成分和机械性能的比较 — 请始终根据适用于您应用的相关规范验证适用性。
根据您的应用场景优化材料选择 - 预约演示
- 72交叉引用
- 5化学成分
- 2机械性能
- 21物理性能
- 1热处理
- -金相组织
- -切削加工性能
- -应力-应变
- -成形性能
- -疲劳
- -断裂
- -爬行
- -焊接接头
- -涂层
- -尺寸
- -摩擦学
- -腐蚀
- -老化
- -耐候性
- -辐照
- 62供应商总数