Titanium Alloy and Selective Laser Melting (SLM)/Effect of HIP post-processing at 850 degrees C/200 MPa in the fatigue behavior of Ti-6Al-4V alloy fabricated by Selective Laser Melting

Genérico · 1 materiais

Designação Grupo do Material
Ti-6Al-4V Titânio chevron_right