Titanium Alloy and Selective Laser Melting (SLM)/Effect of HIP post-processing at 850 degrees C/200 MPa in the fatigue behavior of Ti-6Al-4V alloy fabricated by Selective Laser Melting
Jenerik · 1 malzeme
| Tanım | Malzeme grubu | |
|---|---|---|
| Ti-6Al-4V | Titanyum | chevron_right |