PROPRIETARY Uddeholm Caldie Aceros para herramientas
Actualizaciones de datos
Este material cuenta con 47 propiedades — aquí solo se muestra una parte.
Accede a todas las propiedades del material, incluyendo valores detallados según temperatura y condiciones.
Se requiere registro gratuito • Acceso inmediato
PROPRIETARY Uddeholm Caldie Composición química
Böhler-Uddeholm AG, Product Data Sheets,
¿Buscas datos completos de desempeño de materiales?
Se requiere registro gratuito • Acceso inmediato
PROPRIETARY Uddeholm Caldie Propiedades físicas
Temperatura
Este material cuenta con 47 propiedades — aquí solo se muestra una parte.
Consulta propiedades físicas detalladas en distintas temperaturas y condiciones.
Se requiere registro gratuito • Acceso inmediato
PROPRIETARY Uddeholm Caldie Tratamiento Térmico
- Soft annealing: Protect the steel and heat through to 820°C (1510°F) wait for equalization of the temperature (equalization time related to the size of the tool). Then cool in the furnace at 10°C (20°F) per hour to 650°C (1200°F), then freely in air to room temperature;
Stress relieving: After rough machining the residual stresses should be relieved by tempering at 650°C (1200°F), holding time 2 hr. Cool slowly in the furnace to 500°C (930°F), then freely in air to room temperature;
Hardening: Preheating temperature: 600-650°C (1110–1200°F) and 850-900°C (1560-1650°F). In case of bigger dimensions (> 150 mm cross section) a third preheating step at 930°C (1700°F) is recommended. Austenitizing temperature: 1000-1050°C (1830-1920°F), normally 1020°C (1870°F), in case of bigger dimensions (>150 mm cross section) 1000°C (1830°F). Holding time: 30 min. after the tool is heated through. (Protect the part against decarburization and oxidation.);
Quenching media: Vacuum (high speed gas with sufficient overpressure minimum 2 bar). Martempering bath or fluidized bed at approx. 200-550°C (390-1020°F), forced air/gas. Temper the tool as soon as its temperature reaches 50-70°C (120-160°F);
Tempering: Choose the tempering temperature according to the hardness required by reference to the tempering graph below. Temper at least twice with intermediate cooling to room temperature. For high dimensional stability a minimum temperature of 540°C (1000°F) and three tempers is strongly recommended. If lowering the tempering temperature, it should not be below 520°C (970°F). When tempering twice the minimum holding time at temperature is 2 hours. When tempering three times the minimum holding time is 1 hour. - Austenitizing temperature 1025°C (1880°F). Holding time 30 mintues.
PROPRIETARY Uddeholm Caldie Propiedades mecánicas
Temperatura
¿Buscas información completa sobre propiedades mecánicas para tomar la mejor decisión?
Obtén información completa sobre resistencia, dureza, fatiga y más.
Se requiere registro gratuito • Acceso inmediato
Optimiza la selección de materiales para tu aplicación - Reservar una demo
- -Referencias cruzadas
- 6Composición
- 21Propiedades mecánicas
- 12Propiedades físicas
- 2Tratamiento térmico
- -Metalografía
- -Maquinabilidad
- 1Esfuerzo-Deformación
- -Conformabilidad
- -Fatiga
- -Fractura
- -Bicho raro
- -Uniones
- -Revestimientos
- -Dimensiones
- -Tribología
- -Corrosión
- -Envejecimiento
- -Resistencia a la intemperie
- -Irradiación
- 5Proveedores Totales