ASD-STAN TI-P99001 Titanium Alloys
Data updates
This material has 28 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASD-STAN TI-P99001 Chemical Composition
prEN 3497: 1993 / Aerospace series; Titanium TI-P99001; Annealed; Sheet and strip, cold rolled; a ≤ 6 mm; 290 MPa ≤ Rm ≤ 420 MPa
Looking for full material performance data?
Free registration required • Instant access
ASD-STAN TI-P99001 Physical Properties
Temperature
This material has 28 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASD-STAN TI-P99001 Heat Treatments
- Annealed at 600-840°C, for t ≥ 1 min, air cooled or inert atmosphere.
ASD-STAN TI-P99001 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASD-STAN TI-P99001 International Equivalent Materials
Showing 8 of 8 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 8 international equivalents?
See all 8 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 8Cross References
- 8Composition
- 3Mechanical Properties
- 2Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- 1Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 5Total Suppliers