WL 2.4654 Nickel Alloys
Data updates
This material has 208 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
WL 2.4654 Chemical Composition
WL 2.4654: 1981 / High temperature nickel alloy with about 0.06 C - 19 Cr - 14 Co - 4 Mo - 3 Ti - 1.4 Al; rods and forgings
Looking for full material performance data?
Free registration required • Instant access
WL 2.4654 Physical Properties
Temperature
This material has 208 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
WL 2.4654 Heat Treatments
- Normalized: solution annealing (1150+/-20°C) 4 h/water or oil. Normalized: (800+/-10°C) 4 h/air and aging (760+/-10°C) 16 h/air .
WL 2.4654 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
WL 2.4654 International Equivalent Materials
Showing 15 of 75 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 75 international equivalents?
See all 75 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 75Cross References
- 15Composition
- 15Mechanical Properties
- 34Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 1Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- 1Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 66Total Suppliers