AA 6005A Aluminium Alloys
Data updates
This material has 316 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AA 6005A Chemical Composition
International alloy designations and chemical composition limits for wrought aluminum and wrought aluminum alloys - Teal Sheets (2025), 2025
Looking for full material performance data?
Free registration required • Instant access
AA 6005A Physical Properties
Temperature
This material has 316 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AA 6005A Heat Treatments
- The times and temperatures are typical for various forms, sizes and methods of manufacture and may not exactly describe the optimum treatment for a specific item.
The nominal temperatures at which metal is heated (applies both for solution and precipitation heat treatment) should be attained as rapidly as possible and maintained ± 5°C of nominal during the time at temperature.
The time at precipitation heat treatment temperature will depend on time required for load to reach temperature. The times shown are based on rapid heating, with soaking time measured from the time the load reached within 5°C of the applicable temperature.
Material should be quenched from the solution heat-treating temperature as rapidly as possible and with minimum delay after removal from the furnace. Quenching is typically performed by immersion of wrought products in a cold water bath, although some forgings are quenched in hot-water. Quenching may be performed by alternative means such as total immersion in an aqueous polymer solution, liquefied gas, hot water, or boiling water, or by air blast or fog to minimize distortion provided samples from the material. The use of high-velocity high-volume jets of cold water is also effective for some materials.
For extruded rod, bar, profiles and tubes
Temper T1: Quenched directly from the extrusion press, naturally aged. Some extrusions may be adequately quenched using a room temperature air blast.
Temper T4: Solution heat treated at 510°C, quenched, naturally aged. By suitable control of extrusion temperature, product may be quenched directly from extrusion press to provide specified properties for this temper. Some products may be adequately quenched in air blast at room temperature. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Temper T5: Quenched directly from the extrusion press, precipitation heat treated at 175° for 8 hours. Some extrusions may be adequately quenched using a room temperature air blast.
Temper T61: Solution heat treated at 510°C, quenched, precipitation heat treated at 175° for 8 hours. By suitable control of extrusion temperature, product may be quenched directly from extrusion press to provide specified properties for this temper. Some products may be adequately quenched in air blast at room temperature. By definition, this temper designation is that which would apply after natural aging even though mechanical properties for this alloy-temper product have not been registered.
Annealing (O)
Heated at 415°C, held for 2-3 hours. This treatment is intended to remove effects of solution heat treatment and include cooling at a rate of about 30°C per hour from the annealing temperature to 260°C. The rate of subsequent cooling is unimportant. Treatment at 345°C, followed by uncontrolled cooling, may be used to remove the effects of cold work, or to partially remove the effects of heat treatment. By definition, this temper designation is that which would apply after annealing even though mechanical properties for this alloy temper product have not been registered.
AA 6005A Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AA 6005A International Equivalent Materials
Showing 15 of 127 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 127 international equivalents?
See all 127 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 127Cross References
- 24Composition
- 30Mechanical Properties
- 26Physical Properties
- 1Heat Treatment
- 1Metallography
- -Machinability
- 10Stress-Strain
- -Formability
- 2Fatigue
- -Fracture
- -Creep
- 4Joints
- -Coatings
- -Dimensions
- -Tribology
- 1Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 90Total Suppliers