PROPRIETARY Uddeholm Skolvar Tool steels

Material group: Ferrous Alloys / Tool steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: -
Total number of updates: 0

This material has 12 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Skolvar Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.7
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
5.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.45
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

Uddeholms AB, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Skolvar Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.72 — 8 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 12 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Uddeholm Skolvar Heat Treatments


  • Soft Annealing
    Protect the steel and heat through to 850°C (1560°F). Then cool in furnace at 10°C (20°F) per hour to 600°C (1110°F), then freely in air.
    Stress Relieving
    After rough machining the tool should be heated through to 650°C (1200°F), holding time 2 hours. Cool slowly to 500°C (930°F), then freely in air.
    Hardening
    Preheating temperature: 600 - 650°C (1110 - 1200°F) and 850 - 900°C (1560 - 1650°F). Austenitizing temperature: 1050 - 1150°C (1920 - 2100°F), normally 1050°C (1920°F) or 1130°C (2066°F). Holding time: 30 minutes (<1100°C) or 10 minutes (≥1100°C). Protect the tool against decarburization and oxidation during austenitizing.
    Quenching Media
    High speed gas/circulating atmosphere, vacuum furnace (high speed gas with sufficient overpressure). Temper the tool as soon as its temperature reaches 50 - 70°C (120 - 160°F). To obtain the optimum properties for the tool, the cooling rate should be as fast as possible with regards to acceptable distortion.
    Tempering
    Choose the tempering temperature according to the hardness required. Temper at least twice with intermittent cooling to room temperature. High temperature tempering >525°C (980°F) is recommended whenever possible.
  • Austenitizing temperature 1050°C (1922°F). Holding time 30 minutes.

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 6Composition
  • -Mechanical Properties
  • 3Physical Properties
  • 3Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • -Total Suppliers