8CrMo16-5 (Germany / DIN) Material Properties

Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2021-10
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 800 — 1000 MPa view details
Elongation, A 14 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Brinell Hardness (HB) ≤ 220 view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 116 — 145 ksi view details
Elongation, A 14 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details
Brinell Hardness (HB) ≤ 220 view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.04 – 0.12
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
3.70 – 4.30
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.2500
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

EN ISO 683-5: 2017 / Heat treatable steels, alloy steels and free-cutting steels - Part 5: Nitriding steels

Heat Treatments

  • The base composition and the heat treatment (quenching and tempering) prior to nitriding both have an influence on the results of nitriding treatment. The tempering temperature should not be less than 50°C higher than the nitriding temperature. A difference of less than 50°C should be the subject of a special agreement. <br /> Soft annealing at 640-660°C; <br /> Hardening at 940-960°C (time for austenitizing as a guide: 0.5h minimum) and quenching in water; <br /> Tempering at 620-660°C (time for tempering as a guide: 1h minimum; With very large sizes, the tempering temperature may be agreed at the time of enquiry and order).