TCVN X1CrNi25-21 Stainless steels
Data updates
This material has 154 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
TCVN X1CrNi25-21 Chemical Composition
TCVN 10356: 2014 / Stainless steels − Chemical composition
Looking for full material performance data?
Free registration required • Instant access
TCVN X1CrNi25-21 Physical Properties
Temperature
This material has 154 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
TCVN X1CrNi25-21 Heat Treatments
- Hot forming: heated at 1150-850°C, cooled in air; Solution annealing: heated at 1030-1110°C, quenched in water or rapidly cooled in air.
TCVN X1CrNi25-21 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
TCVN X1CrNi25-21 International Equivalent Materials
Showing 15 of 65 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 65 international equivalents?
See all 65 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 65Cross References
- 18Composition
- 19Mechanical Properties
- 4Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 47Total Suppliers