17SMn20 (European Union / EN) Material Properties

Other designations:
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: European Union / EN

Data updates

Latest Update: 2024-12
Total number of updates: 3
Update History:
2018-10 2018-09

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 420 — 840 MPa view details
Elongation, A 6 % view details
Brinell Hardness (HB) ≤ 181 view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 60.9 — 121.8 ksi view details
Elongation, A 6 % view details
Brinell Hardness (HB) ≤ 181 view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.14 – 0.20
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
1.20 – 1.60
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.060
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

EN 10277: 2018 / Bright steel products - Technical delivery conditions

Heat Treatments

  • Carburizing: 880-980°C. The carburizing temperature will depend on the chemical composition of the steel, the mass of the product, and the carburizing medium. If the steels are direct hardened, in general a temperature of 950°C is not exceeded. For special procedures, for example under vacuum, higher temperatures, for example 1020°C to 1050°C, are not unusual; <br> Direct and simple hardening: 830-870°C; <br> Double hardening: Core-hardening: 880-920°C and case-hardening: 780-820°C; Quenching agent: water, oil, emulsion (depends, for example, on the shape of the products, the cooling conditions and the quantity of furnace filling); <br> Tempering: 150-200°C (1h minimum).