PROPRIETARY WM A-8 Tool steels

Material group: Ferrous Alloys / Tool steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2018-07
Total number of updates: 2
Update History
2018-05

This material has 60 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY WM A-8 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.55
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
5.00
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.30
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
W
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-33-7

Ellwood Specialty Steel, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY WM A-8 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.72 — 8 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 60 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY WM A-8 Heat Treatments


  • Preheating: Heat at a rate not exceeding 400°F per hour to 1400-1450°F and equalize.
    Austenitizing (high heat): Heat slowly from the preheat. Furnace or Salt: 1825-1850°F. Soak for 30 minutes for the first inch of thickness, plus 15 minutes for each additional inch.
    Quenching: Air, pressurized gas, or interrupted oil to 150-125°F. Note: Sizes over 5 inches in cross section may not achieve full hardness by cooling in still air. It is usually necessary to increase the quench cooling rate between 1400 to 900°F by using an air blast, pressurized gas, or an interrupted oil quench. For the oil quench, quench until black, about 900°F, then cool in still air to 150-125°F.
    Tempering: Temper immediately after quenching. Hold temperature for 1 hour per inch of thickness, 2 hours minimum, then air cool to ambient temperature. The typical tempering range is 300 to 600°F. Double tempering is recommended for tempering temperatures of 900°F and higher. To minimize internal stresses in cross sections greater than 6 inches and to improve stability in tools that will be EDM’d after heat treatment, a soaking time of 4 to 6 hours at the tempering temperature is strongly recommended. Cryogenic Treatment: Some prefer to do cryogenic treatment as an extension of the quench from the austenitizing treatment. Others prefer to cryogenically treat after tempering.
    Annealing: Annealing must be performed after hot working and before rehardening. Heat at a rate not exceeding 400°F per hour to 1550°F, and hold at temperature for 1 hour per inch of maximum thickness; 2 hours minimum. Then cool slowly with the furnace at a rate not exceeding 50°F per hour to 1000°F Continue cooling to ambient temperature in the furnace or in air. The resultant hardness should be a maximum of 241 HBW.

PROPRIETARY WM A-8 Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
710 — 2048 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
9 — 24 %
Unlock full details
Full data available with free access View Complete Material Data
Impact Energy
val1
Full data available with free access View Complete Material Data
J
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
448 — 1724 MPa
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

PROPRIETARY WM A-8 International Equivalent Materials


Showing 1 of 1 results.

MATERIAL
STANDARD
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Composition 100%

Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.

Need the full list of 1 international equivalents?

See all 1 equivalent grades with detailed mapping by standard, producer and equivalence category.

View All Equivalents ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 1Cross References

  • 6Composition
  • 42Mechanical Properties
  • 7Physical Properties
  • 2Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 2Total Suppliers