PROPRIETARY Böhler-Uddeholm Holder Structural and constructional steels
Material group:
Ferrous Alloys / Structural and constructional steels
Country / Standard:
PROPRIETARY
Data updates
Latest Update: 2017-07
Total number of updates: 1
Update History
This material has 14 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Böhler-Uddeholm Holder Physical Properties
Temperature
Modulus of Elasticity
190 — 210
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
7.67 — 7.86
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access
View Complete Material Data
This material has 14 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Böhler-Uddeholm Holder Heat Treatments
- It is intended for use in the hardened and tempered condition, i.e., the delivery condition.
Stress Tempering: After rough machining, the tool should be heated through to 900°F, and held for a minimum of 2 hours once the entire tool is soaked through. Cool slowly to room temperature. Stress tempering temperatures in excess of 900°F may result in a permanent loss of strength, hardness, and/or dimensional tolerances.
Flame and induction hardening: Can be flame or induction hardened to a hardness of approx. 50 RC. Cooling in air is preferable. Smaller pieces may however require forced cooling. Hardening should be immediately followed by tempering.
Gasnitriding: Nitriding gives a hard surface which is very resistant to wear and erosion. A nitrided surface also increases the corrosion resistance. The surface hardness after nitriding at a temperature of 525°C in ammonia gas will be approx. 650HV.
PROPRIETARY Böhler-Uddeholm Holder Mechanical Properties
Temperature
Tensile Strength
1010
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Brinell Hardness (HB)
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- -Composition
- 9Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 1Total Suppliers