MS JN/HBW555XCr21 Cast irons
Data updates
This material has 308 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
MS JN/HBW555XCr21 Chemical Composition
MS ISO 21988: 2007 / Abrasion-resistant cast irons - Classification
Looking for full material performance data?
Free registration required • Instant access
MS JN/HBW555XCr21 Heat Treatments
- Typical heat treatments are hardening, tempering, soft annealing and annealing.
A typical hardening cycle is: slowly heating up to a temperature within the range of 900°C to 1050°C, holding for a determined period of time and then rapidly cooling.
A typical tempering cycle involves: slowly heating up to a temperature within the range of 200°C to 550°C, holding for a period of time appropriate to the thickness, followed by air or furnace cooling.
If casting hardness below HBW 378 is required (e.g. to facilitate machining), soft annealing can be carried out. An example of a soft annealing method is: slowly heating up to a temperature within the range of 920°C to 975°C, holding for at least 1 h, then slowly cooling down in the furnace to about 810°C and then further cooling down to 600 °C at a rate not exceeding 55 K/h, followed by air or furnace cooling.
If castings require annealing then a typical annealing involves slowly heating up to a temperature of 700 °C to 750 °C for a minimum of 4 h, and then slowly cooling in the furnace to 600 °C, following by air or furnace cooling.
MS JN/HBW555XCr21 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
MS JN/HBW555XCr21 International Equivalent Materials
Showing 15 of 213 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 213 international equivalents?
See all 213 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 213Cross References
- 9Composition
- 1Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 84Total Suppliers