GB T23352 Tool steels
Data updates
This material has 221 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
GB T23352 Chemical Composition
GB/T 1299: 2025 / Tool and mould steels
Looking for full material performance data?
Free registration required • Instant access
GB T23352 Physical Properties
Temperature
This material has 221 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
GB T23352 Heat Treatments
- Preheated at 790 +/- 15°C. Salt bath at 1010°C or furnace atmosphere at 1020 +/- 6°C, 5 - 15min., oil cooled. Heat treated at 550 +/- 6°C, 2h.
GB T23352 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
GB T23352 International Equivalent Materials
Showing 15 of 104 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 104 international equivalents?
See all 104 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 104Cross References
- 16Composition
- 2Mechanical Properties
- 4Physical Properties
- 1Heat Treatment
- 1Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 1Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 92Total Suppliers