VdTÜV 12 CrMo 19 5 Structural and constructional steels

Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / VdTÜV

Data updates

Latest Update: -
Total number of updates: 0
Update History

This material has 515 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

VdTÜV 12 CrMo 19 5 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.04 – 0.17
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
3.90 – 6.10
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.26 – 0.64
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

WB 007/1: 2001 / Hydrogen-resistant and heat-resistant steel 12 CrMo19 5 G and 12 CrMo 19 5 V, material no. 1.7362

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

VdTÜV 12 CrMo 19 5 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.67 — 7.86 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 515 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

VdTÜV 12 CrMo 19 5 Heat Treatments

  • Annealed (G): 880-920°C, cooled in the furnace 720-680°C (at least 60 min), cooled in air. Hardened and tempered (V): Hardened - 930 to 980°C, cooled in air, in oil or water. Tempered: 680-760°C, cooled in air.
  • Annealed (G): 880-920°C, cooled in the furnace 720-680°C (at least 60 min), cooled in air; Hardened and tempered (V): Hardened - 930 to 980°C, cooled in air, in oil or water. Tempered: 680-760°C, cooled in air.

VdTÜV 12 CrMo 19 5 Mechanical Properties


Temperature

PROPERTY / VALUE
Yield Strength, Rp0.2
155 MPa
Unlock full details
Full data available with free access View Complete Material Data
Tensile Strength
395 — 750 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
16 %
Unlock full details
Full data available with free access View Complete Material Data
Impact Energy
val1
Full data available with free access View Complete Material Data
J
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book a Demo

  • 209 Cross References

  • 14 Composition
  • 81 Mechanical Properties
  • 3 Physical Properties
  • 2 Heat Treatment
  • - Metallography
  • - Machinability

  • - Stress-Strain
  • - Formability
  • - Fatigue
  • - Fracture
  • 4 Creep

  • 18 Joints
  • - Coatings
  • - Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 184 Total Suppliers