1.2067 (Germany / DIN) Material Properties

Other designations: , ,
Material group: Ferrous Alloys / Structural and constructional steels, Ferrous Alloys / Tool steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2023-10
Total number of updates: 6
Update History:
2021-12 2019-06 2019-05 2019-03 2018-11

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 750 MPa view details
Elongation, A 11 % view details
Brinell Hardness (HB) ≤ 225 view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 108.8 ksi view details
Elongation, A 11 % view details
Brinell Hardness (HB) ≤ 225 view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 212 GPa view details
Shear Modulus val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 33 W/(m∙°C) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Electrical Resistivity 0.3 Ω∙mm²/m view details
Modulus of Elasticity 27.6 E+03 — 30.7 E+03 ksi view details
Shear Modulus val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 19.1 BTU/(h∙ft∙°F) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Electrical Resistivity 499 E-06 Ω∙circular·mil/ft view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.9500 – 1.1000
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.3500 – 1.6500
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.2500 – 0.4500
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

DIN 17350: 1980 / Tool Steels; Technical Conditions of Delivery

Heat Treatments

  • <b>Soft annealing</b>: Slowly heated at 710-750°C, held for several hours, slowly cooled, preferably in the furnace. <br />The soft annealing is most appropriate for machining and cold working and provides the most favorable initial structure for tool hardening.<br /><br /><b>Hardening</b>: Preheated at 500-600°C and then heated faster at 830-860°C, quenched in oil. <br />Temperature of oil should be approx. 50°C. When quenching in aqueous salt solutions, the temperature of the quenching agent may rise to 100°C. <br />Hardening immediately after forging without cooling and annealing is inappropriate because of the risk of cracking. <br /><br /><b>Stress relief annealing</b>: Slowly heated at 600-650°C, held for 1-2 hours, slowly cooled in the furnace.
  • Austenitized at 840 +/- 10°C and oil quenched.<br />Tempered at 180 +/- 10°C.