ASME SA-541 Grade 22 Class 3 Structural and constructional steels
Alternative designations:
2 1/4Cr-1Mo
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
United States / ASME
Data updates
Latest Update: 2024-02
Total number of updates: 5
Update History
2024-01
2023-11
2023-10
2020-10
ASME SA-541 Grade 22 Class 3 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.11 – 0.15
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
2.00 – 2.50
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.30 – 0.60
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
ASME Boiler and Pressure Vessel Code An International Code Section II - Part A Ferrous Material Specifications / American Society of Mechanical Engineers / 2025
Looking for full material performance data?
View Complete Material Data ›ASME SA-541 Grade 22 Class 3 Physical Properties
Temperature
Modulus of Elasticity
val1
Full data available with free access
View Complete Material Data
GPa
Unlock full details
Poisson Coefficient
val1
Full data available with free access
View Complete Material Data
Unlock full details
Coefficient of Thermal Expansion (CTE)
val1
Full data available with free access
View Complete Material Data
10-6/°C
Unlock full details
This material has 190 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
ASME SA-541 Grade 22 Class 3 Heat Treatments
- After complete austenitization, the forgings shall be quenched in a suitable liquid medium by spraying or immersion. Quenching shall be followed by tempering at a subcritical temperature and holding at this temperature for a minimum time of 30 min/25 mm of maximum section thickness. Minimum tempering temperatures shall be 650°C (1200°F).
ASME SA-541 Grade 22 Class 3 Mechanical Properties
Temperature
Reduction of Area
val1
Full data available with free access
View Complete Material Data
%
Unlock full details
Mechanical properties are available with full access.
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›-
10 Cross References
-
9 Composition
-
36 Mechanical Properties
-
85 Physical Properties
-
1 Heat Treatment
-
- Metallography
-
- Machinability
-
1 Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
48 Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
- Total Suppliers