ASTM A 313 S30151 Stainless steels
Data updates
This material has 49 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 313 S30151 Chemical Composition
A313/A313M: 2018 / Standard Specification for Stainless Steel Spring Wire
Looking for full material performance data?
Free registration required • Instant access
ASTM A 313 S30151 Physical Properties
Temperature
This material has 49 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM A 313 S30151 Heat Treatments
- By heat treating the material at 350 - 425°C (660 - 800°F) for 0.5 - 4h, the tensile strength will increase by approximately 150 - 300 MPa. If a shorter heat treatment time is used, the effect will be less.
ASTM A 313 S30151 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 313 S30151 International Equivalent Materials
Showing 7 of 7 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 7 international equivalents?
See all 7 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 7Cross References
- 10Composition
- 19Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 4Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 5Total Suppliers