1.7710 (Germany / DIN) Material Properties

Other designations:
Material group: Ferrous Alloys / Cast steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2015-01
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
≥ 300°C
PROPERTY / VALUE
Yield Strength, Rp0.2 700 MPa view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 850 — 1150 MPa view details
Elongation, A 6 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 101.5 ksi view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 123.3 — 166.8 ksi view details
Elongation, A 6 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.12 – 0.18
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.30 – 1.80
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2

EN 10293: 2015 / Steel castings for general engineering uses

Heat Treatments

  • Quenched and tempered: (+QT1) quenched from 950 to 980°C, cooled in liquid (for information only) and tempered from 650 to 670°C;<br />(+QT2) from quenched from 950 to 980°C, cooled in liquid (for information only) and tempered from 610 to 640°C.