MSZ G 15 CrMoV 6-9 Cast steels
Data updates
This material has 107 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
MSZ G 15 CrMoV 6-9 Chemical Composition
EN 10293: 2015 / Steel castings for general engineering uses
Looking for full material performance data?
Free registration required • Instant access
MSZ G 15 CrMoV 6-9 Heat Treatments
- Quenched and tempered: (+QT1) quenched from 950 to 980°C, cooled in liquid (for information only) and tempered from 650 to 670°C;
(+QT2) from quenched from 950 to 980°C, cooled in liquid (for information only) and tempered from 610 to 640°C.
MSZ G 15 CrMoV 6-9 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
MSZ G 15 CrMoV 6-9 International Equivalent Materials
Showing 15 of 40 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 40 international equivalents?
See all 40 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 40Cross References
- 10Composition
- 16Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 40Total Suppliers