EN 30 NiCrMo 16-6 Structural and constructional steels
Data updates
This material has 431 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
EN 30 NiCrMo 16-6 Chemical Composition
EN 10083-3: 2006 / Steels for quenching and tempering - Part 3: Technical delivery conditions for alloy steels
Looking for full material performance data?
Free registration required • Instant access
EN 30 NiCrMo 16-6 Physical Properties
Temperature
This material has 431 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
EN 30 NiCrMo 16-6 Heat Treatments
- Austenitizing (quenching in oil): 840-860°C, (at least 30 min). NOTE: The temperatures at the lower end of the range are generally applicable to hardening in water and those at the upper end for hardening in oil. Synthetic quenchants may also be used; Tempering: 540-630°C, (at least 60 min); End quench test: 850±5°C.
- Hardened: 840-860°C / OQ + Tempered: >=525°C / OQ.
EN 30 NiCrMo 16-6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
200 Cross References
-
16 Composition
-
33 Mechanical Properties
-
3 Physical Properties
-
3 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
4 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
172 Total Suppliers