36Mn6 (Japan / JIS) Material Properties
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
Japan / JIS
Data updates
Latest Update: -
Total number of updates: 0
Update History:
-
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.33 – 0.40
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
1.30 – 1.65
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.035
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
G 7105: 2000 / Heat-treatable steels, alloy steels and free-cutting steels - Part 18: Bright products of unalloyed and low alloy steels
Heat Treatments
- TC+TA - cold drawn and annealed to maximum hardness requirements. P+TA - peeled and annealed to maximum hardness requirements. G+TA - ground and annealed to maximum hardness requirements. TC+TQ+TT - cold drawn and quenched + tempered. P+TQ+TT - peeled and quenched + tempered. G+TQ+TT - ground and quenched + tempered. Hardening: 830-870°C (1/2 hour), water or oil quench; Tempering: 540-680°C (1 hour).
- Water or oil quenching: 820-860°C (1/2 hour), Tempering: 540-680°C (1 hour).
-
76 Cross References
-
10 Composition
-
60 Mechanical Properties
-
3 Physical Properties
-
3 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
19 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
47 Total Suppliers