B.S. 1.6771 Cast steels
Data updates
This material has 201 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
B.S. 1.6771 Chemical Composition
EN 10293: 2015 / Steel castings for general engineering uses
Looking for full material performance data?
Free registration required • Instant access
B.S. 1.6771 Heat Treatments
- Quenched and tempered: (+QT1) quenched from 820 to 880°C, cooled in liquid or air (for information only) and tempered from 600 to 680°C;
(+QT2) quenched from 820 to 880°C, cooled in liquid or air (for information only) and tempered from 550 to 600°C.
B.S. 1.6771 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
B.S. 1.6771 International Equivalent Materials
Showing 15 of 88 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 88 international equivalents?
See all 88 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 88Cross References
- 10Composition
- 20Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 82Total Suppliers