DIN 1.6570 Cast steels

Material group: Ferrous Alloys / Cast steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2021-03
Total number of updates: 5
Update History
2020-04 2019-06 2018-12 2016-04

This material has 304 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.6570 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.2700 – 0.3400
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
1.1000 – 1.4000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.6000 – 1.0000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

DIN 17205: 1992 / Quenched and tempered steel castings for general applications; technical delivery conditions

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.6570 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
211 GPa
Unlock full details
Full data available with free access View Complete Material Data

This material has 304 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.6570 Heat Treatments

  • Quenched at ≤ 920°C
    Tempered at 600-650°C
    Stress relief annealed at ≥ 570°C. This temperature must be at least 30°C below the tempering temperature and must not be below the specified minimum value
  • Air Quenched and Tempered Hardening: 880-920°C; Tempering: 600-650°C Liquid Quenched and Tempered (I) Hardening: 880-920°C; Tempering: 600-650°C Liquid Quenched and Tempered (II) Hardening: 880-920°C; Tempering: 500-550°C

DIN 1.6570 Mechanical Properties


Temperature

PROPERTY / VALUE
Yield Strength, Rp0.2
550 MPa
Unlock full details
Full data available with free access View Complete Material Data
Tensile Strength
750 — 1250 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
8 %
Unlock full details
Full data available with free access View Complete Material Data
Impact Energy
val1
Full data available with free access View Complete Material Data
J
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book a Demo

  • 90 Cross References

  • 26 Composition
  • 62 Mechanical Properties
  • 7 Physical Properties
  • 3 Heat Treatment
  • - Metallography
  • - Machinability

  • 15 Stress-Strain
  • - Formability
  • 15 Fatigue
  • - Fracture
  • - Creep

  • - Joints
  • - Coatings
  • - Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 86 Total Suppliers