X105CrMo17 (Hungary / MSZ) Material Properties

Other designations: ,
Material group: Ferrous Alloys / Stainless steels
Country/Standard: Hungary / MSZ

Data updates

Latest Update: 2020-03
Total number of updates: 9
Update History:
2017-07 2017-01 2016-11 2015-02 2015-01 2014-10 2014-09 2014-07

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Brinell Hardness (HB) ≤ 285 view details
Rockwell Hardness (HR) 54 — 60 view details
Vickers Hardness (HV) 590 — 720 view details
Brinell Hardness (HB) ≤ 285 view details
Rockwell Hardness (HR) 54 — 60 view details
Vickers Hardness (HV) 590 — 720 view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 215 GPa view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 15 W/(m∙°C) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Electrical Resistivity 0.8 Ω∙mm²/m view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/m
view details
Modulus of Elasticity 27.6 E+03 — 31.2 E+03 ksi view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 8.67 BTU/(h∙ft∙°F) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Electrical Resistivity 481 Ω∙circular·mil/ft view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/in
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.95 – 1.20
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
16.0 – 18.0
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
≤ 1.00
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

EN 10088-1: 2023 / Stainless steels - Part 1: List of stainless steels

Heat Treatments

  • Hardened and tempered: + (1030 to 1070) ± 10°C / OQ (may be sub-zero treated at - 80°C ± 10°C)+ temper θ >= 140 °C ± 10 °C.
  • Hot formed at 1100 to 800°C, slow cooled. <br> Softened at 750 to 780°C, cooled in oven. <br> Austenitic heat treatment (solvent, heat treatment) at 1000 to 1050°C, cooled in oil or air.<br> Tempered at 100 to 200°C, cooled in air or oil.