UNI 1 C 22 Chemical Composition
EN 10083-2: 1991 / Steels for quenching and tempering - Part 2: Technical delivery conditions for non alloy steels
Looking for full material performance data?
Free registration required • Instant access
UNI 1 C 22 Physical Properties
Temperature
This material has 9052 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
UNI 1 C 22 Heat Treatments
- Austenitizing (quenching in water): 860-900°C (30 min.); Tempering: 550-660°C (60 min.); Normalizing: 880-920°C (30 min.)
UNI 1 C 22 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
UNI 1 C 22 International Equivalent Materials
Showing 15 of 227 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 227 international equivalents?
See all 227 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 227Cross References
- 9Composition
- 92Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 83Joints
- -Coatings
- 4Dimensions
- 1Tribology
- 8491Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 141Total Suppliers