Mechanical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.17 – 0.24
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.40
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cr+Mo+Ni
VALUE
≤ 0.63
UNIT
%
CAS NUMBER
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

Steels for quenching and tempering - Part 2: Technical delivery conditions for non alloy steels, EN 10083-2 / 1991

Heat Treatments

  • Austenitizing (quenching in water): 860-900°C (30 min.); Tempering: 550-660°C (60 min.); Normalizing: 880-920°C (30 min.)