IS XT110Mo10Co8Cr4W2 Tool steels
Data updates
This material has 122 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
IS XT110Mo10Co8Cr4W2 Chemical Composition
IS 7291: 1981 / High speed tool steels
Looking for full material performance data?
Free registration required • Instant access
IS XT110Mo10Co8Cr4W2 Physical Properties
Temperature
This material has 122 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
IS XT110Mo10Co8Cr4W2 Heat Treatments
- Annealed: 860°C, rate of cooled: 15°C/h. Preheted: 850°C; hardened: 1180-1230°C, 2-5 min, oil, air or salt cooled; tempered: 530-570°C. Forging temperature range: 950-1150°C.
IS XT110Mo10Co8Cr4W2 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
IS XT110Mo10Co8Cr4W2 International Equivalent Materials
Showing 15 of 55 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 55 international equivalents?
See all 55 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 55Cross References
- 10Composition
- 3Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 50Total Suppliers