IS 42Cr4Mo2 Structural and constructional steels
Data updates
This material has 509 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
IS 42Cr4Mo2 Chemical Composition
IS 3930: 1994 / Flame and induction hardening steels
Looking for full material performance data?
Free registration required • Instant access
IS 42Cr4Mo2 Physical Properties
Temperature
This material has 509 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
IS 42Cr4Mo2 Heat Treatments
- Hot worked temperature: 1200-850°C. Normalized: 850-880°C. Hardened: 850-880°C. Quenched medium: oil. Tempered: 500-720°C.
- Hot worked: 850-1200°C. Soft annealed: 650-700°C. Hardened: 830-860°C, oil quench; tempered: 530-670°C. Hardened: 840-870°C, water quench; tempered: 530-670°C.
IS 42Cr4Mo2 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
IS 42Cr4Mo2 International Equivalent Materials
Showing 15 of 282 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 282 international equivalents?
See all 282 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 282Cross References
- 36Composition
- 89Mechanical Properties
- 3Physical Properties
- 7Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 32Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 60Total Suppliers