PROPRIETARY Uddeholm Orvar 2 Microdized Tool steels
Data updates
This material has 75 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY Uddeholm Orvar 2 Microdized Chemical Composition
Uddeholms AB, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY Uddeholm Orvar 2 Microdized Physical Properties
Temperature
This material has 75 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY Uddeholm Orvar 2 Microdized Heat Treatments
- Soft annealing: Protect the steel and heat through to 850°C (1562°F). Then cool in the furnace at 10°C (18°F) per hour to 650°C (1202°F), then freely in air;
Stress relieving: After rough machining the tool should be heated through to 650°C (1202°F), holding time 2 hours. Cool slowly to 500°C (932°F), then freely in air;
Hardening: Pre-heating temperature: 600-850°C (1112-1562°F), normally in two pre-heating steps. Austenitizing temperature: 1020-1050°C (1868-1922°F), normally 1020-1030°C (1868-1886°F);
Quenching media: High speed gas/circulating atmosphere, Vacuum (high speed gas with sufficient positive pressure). An interrupted quench is recommended where distortion control and quench cracking are a concern, Martempering bath or fluidized bed at 450-550°C (842-1022°F), then cool in air, Martempering bath or fluidized bed at 180-220°C (356-428°F) then cool in air, Warm oil;
Tempering: Choose the tempering temperature according to the hardness required by reference to the tempering graph. Temper minimum twice with intermediate cooling to room temperature. Lowest tempering temperature 250°C (482°F). Holding time at temperature minimum 2 h.
Nitriding and Nitrocarburizing:
Gas nitriding at 510°C for 10 h and 0.12 mm depth or 30 h for 0.20 mm depth.
Plasma nitriding at 480°C for 10 h and 0.12 mm depth or 30 h for 0.18 mm depth.
Nitrocarburizing in gas at 580°C for 2.5 h and 0.11 mm depth or in salt bath at 580°C for 1 h and 0.06 mm depth. - Austenitizing temperature 1020°C (1870°F). Holding time 30 min
PROPRIETARY Uddeholm Orvar 2 Microdized Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PROPRIETARY Uddeholm Orvar 2 Microdized International Equivalent Materials
Showing 2 of 19 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 19 international equivalents?
See all 19 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 19Cross References
- 6Composition
- 26Mechanical Properties
- 14Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 2Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 6Total Suppliers