ISO HS6-5-2C Tool steels
Data updates
This material has 178 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ISO HS6-5-2C Chemical Composition
ISO 4957: 2018 / Tool steels
Looking for full material performance data?
Free registration required • Instant access
ISO HS6-5-2C Physical Properties
Temperature
This material has 178 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ISO HS6-5-2C Heat Treatments
- Austenitized at 1210 ± 10°C and quenched. Usual quenching media in practice are air, gas or salt bath. Total heating time of test pieces in a salt bath is 3 min. for hardening and minimum 2 periods of 60 min. each for tempering.
Tempered at 560 ± 10°C.
ISO HS6-5-2C Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ISO HS6-5-2C International Equivalent Materials
Showing 15 of 101 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 101 international equivalents?
See all 101 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 101Cross References
- 9Composition
- 14Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 6Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 44Total Suppliers