ASTM A 681 Type L6 Tool steels
Data updates
This material has 222 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 681 Type L6 Chemical Composition
A681: 2024 / Standard Specification for Tool Steels Alloy
Looking for full material performance data?
Free registration required • Instant access
ASTM A 681 Type L6 Physical Properties
Temperature
This material has 222 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM A 681 Type L6 Heat Treatments
- Preheat: 649°C (1200°F); Austenitizing: Salt Bath: 816°C (1500°F), Controlled Atmosphere Furnaces: 829°C (1525°F); Austenitizing time: 5-15 minutes; Quench Medium: Oil; Tempering: 204°C (400°F), Single-tempered for 2h
ASTM A 681 Type L6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 681 Type L6 International Equivalent Materials
Showing 15 of 91 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 91 international equivalents?
See all 91 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 91Cross References
- 8Composition
- 3Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 40Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 76Total Suppliers