ASTM A 351 Grade CF8C Cast steels
Data updates
This material has 354 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM A 351 Grade CF8C Chemical Composition
A351/A351M: 2024 / Standard Specification for Castings, Austenitic, for Pressure-Containing Parts
Looking for full material performance data?
Free registration required • Instant access
ASTM A 351 Grade CF8C Heat Treatments
- Heating at min.1065°C (1950°F) followed by a quench in water or rapid cool by other means. Stabilized at 870 - 900°C (1600 - 1650°F) for a minimum time of 1 h/25 mm (1 inch) of thickness and water quenched or rapidly cooled by other means. The grade designation symbol shall be followed by the symbol “S33”.
ASTM A 351 Grade CF8C Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM A 351 Grade CF8C International Equivalent Materials
Showing 15 of 122 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 122 international equivalents?
See all 122 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 122Cross References
- 9Composition
- 48Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- 29Creep
- 46Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 99Total Suppliers