SAE 348 Chemical Composition
SAE J 405: 1998 / Chemical compositions of SAE wrought stainless steels
Looking for full material performance data?
Free registration required • Instant access
SAE 348 Physical Properties
Temperature
This material has 410 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
SAE 348 Heat Treatments
- Annealing: Heating to 982-1121°C (1800-2050°F); air cooling or water quenching. When stress relieving after welding is specified hold for 0.5 hour minimum at 982-1121°C (1800-2050°F) or at 899 ± 13.9°C (1650 ± 25°F) for 2 hours.
SAE 348 International Equivalent Materials
Showing 15 of 297 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 297 international equivalents?
See all 297 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 297Cross References
- 8Composition
- -Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 1Fatigue
- -Fracture
- -Creep
- 1Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 99Total Suppliers