SAE 1020 Structural and constructional steels
Data updates
This material has 2130 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
SAE 1020 Chemical Composition
SAE J403: 2014 / Chemical Compositions of SAE Carbon Steels
Looking for full material performance data?
Free registration required • Instant access
SAE 1020 Physical Properties
Temperature
This material has 2130 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
SAE 1020 Heat Treatments
- Carbonitrided: 900-925°C, cooling in water or caustic; reheat: 790°C, cooling in water or caustic (3% sidium hydroxide); Carbonitrided: 790-900°C, cooling in oil; temper: 120-205°C.
SAE 1020 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
SAE 1020 International Equivalent Materials
Showing 15 of 899 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 899 international equivalents?
See all 899 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 899Cross References
- 32Composition
- 65Mechanical Properties
- 61Physical Properties
- 5Heat Treatment
- 7Metallography
- 4Machinability
- 8Stress-Strain
- 2Formability
- 7Fatigue
- -Fracture
- -Creep
- 268Joints
- -Coatings
- 30Dimensions
- 1Tribology
- 3Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 738Total Suppliers