FCD 900 A (Japan / JIS) Material Properties

Material group: Ferrous Alloys / Cast irons
Country/Standard: Japan / JIS

Data updates

Latest Update: 2017-10
Total number of updates: 2
Update History:
2016-01

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 600 MPa view details
Tensile Strength 900 MPa view details
Elongation, A 8 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 87 ksi view details
Tensile Strength 130.5 ksi view details
Elongation, A 8 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Heat Treatments

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now