EN-GJS-900-8 (European Union / EN) Material Properties

Other designations:
Material group: Ferrous Alloys / Cast irons
Country/Standard: European Union / EN

Data updates

Latest Update: 2016-03
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 800 MPa view details
Elongation, A 3 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Brinell Hardness (HB) 280 — 340 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 116 ksi view details
Elongation, A 3 % view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details
Brinell Hardness (HB) 280 — 340 view details

Physical Properties


Temperature

0 - 30°C
100 - 300°C
PROPERTY / VALUE
Modulus of Elasticity 169 GPa view details
Density 7.1 kg/dm³ view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 20 — 23 W/(m∙°C) view details
Modulus of Elasticity 24.5 E+03 ksi view details
Density 0.257 lb/in³ view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 11.6 — 13.3 BTU/(h∙ft∙°F) view details

Composition

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Heat Treatments

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now