JIS SCCrM 3 Cast steels
Data updates
This material has 207 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
JIS SCCrM 3 Chemical Composition
G 5111: 1991 / High Tensile Strength Carbon Steel Castings And Low Alloy Steel Castings For Structural Purposes
Looking for full material performance data?
Free registration required • Instant access
JIS SCCrM 3 Heat Treatments
- Normalizing shall be carried out at 850 - 950°C, followed by tempering at 550 - 650°C. Quenching shall be carried out from 850 - 950°C, followed by tempering at 550 - 650°C.
JIS SCCrM 3 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
JIS SCCrM 3 International Equivalent Materials
Showing 15 of 107 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 107 international equivalents?
See all 107 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 107Cross References
- 7Composition
- 8Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 84Total Suppliers