UNI X 8 Cr 17 Stainless steels
Data updates
This material has 334 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
UNI X 8 Cr 17 Chemical Composition
UNI 6901: 1971 / Semi-finished products and hot-rolled or forged bars and rods of special alloyed stainless steel, resistant to corrosion and heat
Looking for full material performance data?
Free registration required • Instant access
UNI X 8 Cr 17 Physical Properties
Temperature
This material has 334 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
UNI X 8 Cr 17 Heat Treatments
- Annealed at 750 - 850°C.
- Forging temperature: 1050-750°C; Recrystallization annealing: 760-820°C.
UNI X 8 Cr 17 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
UNI X 8 Cr 17 International Equivalent Materials
Showing 15 of 166 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 166 international equivalents?
See all 166 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 166Cross References
- 28Composition
- 37Mechanical Properties
- 3Physical Properties
- 3Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 97Total Suppliers