AFNOR NF Z 8 CNF 18-09 Stainless steels
Data updates
This material has 501 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF Z 8 CNF 18-09 Chemical Composition
NF A 35-574: 1990 / Iron and steel. Stainless steel for general purposes. Semi - finished products, bars and wire rod
Looking for full material performance data?
Free registration required • Instant access
AFNOR NF Z 8 CNF 18-09 Physical Properties
Temperature
This material has 501 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF Z 8 CNF 18-09 Heat Treatments
- Hyper tempered at 1000 to 1075°C
AFNOR NF Z 8 CNF 18-09 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AFNOR NF Z 8 CNF 18-09 International Equivalent Materials
Showing 15 of 297 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 297 international equivalents?
See all 297 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 297Cross References
- 9Composition
- 31Mechanical Properties
- 13Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 3Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 147Total Suppliers