AFNOR NF XC 32 Structural and constructional steels
Data updates
This material has 654 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF XC 32 Chemical Composition
NF A 37-502: 1984 / Non-alloy carbon (C superior to 0, 25 per cent) steel cold- rolled strip for heat treatment. Qualities
Looking for full material performance data?
Free registration required • Instant access
AFNOR NF XC 32 Physical Properties
Temperature
This material has 654 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF XC 32 Heat Treatments
- Normalized at 850-875°C
Heated in the range at 835-865°C, cooled in water and tempered at 550-650°C - Normalizing at 850- 875°C; Water quenching at 850°C; Tempering at 550°C
AFNOR NF XC 32 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AFNOR NF XC 32 International Equivalent Materials
Showing 15 of 335 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 335 international equivalents?
See all 335 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 335Cross References
- 19Composition
- 55Mechanical Properties
- 3Physical Properties
- 3Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- 1Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 2Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 236Total Suppliers