AFNOR NF X75WCrV18-4-1 Structural and constructional steels
Data updates
This material has 220 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF X75WCrV18-4-1 Chemical Composition
EN ISO 683-17: 2023 / Heat-treatable steels, alloy steels and free-cutting steels - Part 17: Ball and roller bearing steels
Looking for full material performance data?
Free registration required • Instant access
AFNOR NF X75WCrV18-4-1 Physical Properties
Temperature
This material has 220 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AFNOR NF X75WCrV18-4-1 Heat Treatments
- Preheat: 850°C; austenitise: 1220 +/- 20°C; Isothermally quench: 550°C, 5 minutes (air cool); Temper: 550°C, 2 hours.
AFNOR NF X75WCrV18-4-1 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AFNOR NF X75WCrV18-4-1 International Equivalent Materials
Showing 15 of 104 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 104 international equivalents?
See all 104 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 104Cross References
- 19Composition
- 2Mechanical Properties
- 3Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 1Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 89Total Suppliers